纵向静磁场下单晶高温合金定向凝固籽晶回熔界面杂晶的形成与演化 |
| 苏震奇, 张丛江, 袁笑坦, 胡兴金, 芦可可, 任维丽, 丁彪, 郑天祥, 沈喆, 钟云波, 王晖, 王秋良 |
|
Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field |
| SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang |
| 图11 不同磁场强度下胞晶液/固界面附近热电流与热电磁力分布 |
| Fig.11 Distribution of thermoelectric current (a1, b1) and thermoelectro-magnetic force (a2, b2) at the liquid-solid interface of the cellar crystal under different magnetic fields (The red arrows represent the directions of the current) (a1, a2) 0.5 T (b2, b2) 1 T |
|