纵向静磁场下单晶高温合金定向凝固籽晶回熔界面杂晶的形成与演化 |
| 苏震奇, 张丛江, 袁笑坦, 胡兴金, 芦可可, 任维丽, 丁彪, 郑天祥, 沈喆, 钟云波, 王晖, 王秋良 |
|
Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field |
| SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang |
| 图10 计算域和其网格划分:包括液相、固相和胞状液/固界面的计算域及其横截面 |
| Fig.10 Computing domain and its meshing (a) computational domains including liquid, solid, and cellular liquid-solid interfaces (b) cross section, taken from the white curve area in Fig.10a |
|