纵向静磁场下单晶高温合金定向凝固籽晶回熔界面杂晶的形成与演化
苏震奇, 张丛江, 袁笑坦, 胡兴金, 芦可可, 任维丽, 丁彪, 郑天祥, 沈喆, 钟云波, 王晖, 王秋良

Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field
SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang
图6 0.5 T磁场强度下不同抽拉速率时合金经定向凝固后在不同凝固长度处横截面宏观形貌
Fig.6 Macroscopic morphologies of cross section at the directional-solidification lengths of 0 mm (a1-c1), 15 mm (a2-c2), and 35 mm (a3-c3) under 0.5 T magnetic field at the pilling rates of 20 μm/s (a1-a3), 50 μm/s (b1-b3), and 100 μm/s (c1-c3)