镍基单晶高温合金DD432的持久性能各向异性 |
| 张子轩, 于金江, 刘金来 |
|
Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432 |
| ZHANG Zixuan, YU Jinjiang, LIU Jinlai |
| 图6 3种取向样品在不同条件下蠕变断裂后显微组织的SEM像 |
| Fig.6 SEM images of <001> (a, b), <011> (c, d), and <111> (e, f) oriented specimens after creep rupture under 760oC, 810 MPa (a, c, e) and 1000oC, 280 MPa (b, d, f) |
|