镍基单晶高温合金DD432的持久性能各向异性 |
| 张子轩, 于金江, 刘金来 |
|
Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432 |
| ZHANG Zixuan, YU Jinjiang, LIU Jinlai |
| 图4 <001>、<011>和<111>取向样品的蠕变曲线 |
| Fig.4 Tensile creep curves of <001>, <011>, and <111> oriented specimens under 760oC and 810 MPa (a) and 1000oC and 280 MPa (b) (Inset in Fig.4b is the magnification of initial creep curves) |
|