| 张子轩, 于金江, 刘金来 |
|
Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432 |
| ZHANG Zixuan, YU Jinjiang, LIU Jinlai |
| 图3 1000℃、280 MPa条件下持久寿命随取向偏离角度变化统计图 |
| Fig.3 Statistical diagram of the change of stress rupture life with deviation of orientation under 1000oC and 280 MPa |
|