微量Al、Ti对Inconel 690合金高温氧化行为的影响
徐文国, 郝文江, 李应举, 赵庆彬, 卢炳聿, 郭和一, 刘天宇, 冯小辉, 杨院生

Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy
XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng
图6 690、690-Al和690-(Al, Ti)合金在1000℃下氧化100 h后氧化膜截面形貌的SEM像和元素分布
Fig.6 Cross-sectional SEM images and corresponding EDS elemental maps of oxide scale on 690 (a), 690-Al (b), 690-(Al, Ti) (c) alloys after oxidation at 1000oC for 100 h