微量Al、Ti对Inconel 690合金高温氧化行为的影响
徐文国, 郝文江, 李应举, 赵庆彬, 卢炳聿, 郭和一, 刘天宇, 冯小辉, 杨院生

Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy
XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng
图3 690、690-Al和690-(Al, Ti)合金在850、1000和1200℃下氧化100 h后氧化膜表面形貌的SEM像
Fig.3 Surface SEM images of oxide scales of 690 (a, d, g), 690-Al (b, e, h), and 690-(Al, Ti) (c, f, i) alloys after oxidation at 850oC (a-c), 1000oC (d-f), and 1200oC (g-i) for 100 h