表2 1873 K铁液中活度相互作用系数εCPb、εCMn、εMnCr和εAlSi在贡献系数取不同值条件下的计算值εi(Calc.)j与实验值εi(Exp.)j[6]比较
Table 2 Calculated values εi(Calc.)j of activity interaction coefficients εCPb, εCMn, εMnCr, and εAlSi in liquid iron alloy at 1873 K under specified contribution coefficient values, together with the corresponding experimental data εi(Exp.)j from Ref.[6]
k-i-jαi(ij)kαj(ij)kαi(ik)jαj(jk)iεi(Calc.)jεi(Exp.)j
Fe-C-Pb10004.155.73
01001.32
0111-7.56
1011-4.73
1001-1.34
10100.76
0101-4.17
0110-2.07
Fe-C-Mn1000-8.96-1.88
0100-1.62
0111-5.01
1011-12.35
1001-8.96
1010-12.35
0101-1.62
0110-5.01
Fe-Mn-Cr10000.740.90
01000.74
01110.73
10110.74
10010.74
10100.74
01010.73
01100.74
Fe-Al-Si10006.036.97
01006.01
01116.80
10116.82
10016.51
10106.34
01016.49
01106.32