渣-金界面气泡夹带行为数值物理模拟 |
| 周小宾, 赵占山, 汪万行, 徐建国, 岳强 |
|
Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface |
| ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang |
| 图7 渣层中钢液体积随时间的变化 |
| Fig.7 Variations of entrainment volume of molten steel as a function of time |
|