渣-金界面气泡夹带行为数值物理模拟 |
| 周小宾, 赵占山, 汪万行, 徐建国, 岳强 |
|
Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface |
| ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang |
| 图2 计算域及边界条件示意图 |
| Fig.2 Schematic of the computational domain and boundary conditions (d—diameter) |
|