UN核燃料烧结致密化过程的相场模拟 |
| 戚晓勇, 柳文波, 何宗倍, 王一帆, 恽迪 |
|
Phase-Field Simulation of the Densification Process During Sintering of UN Nuclear Fuel |
| QI Xiaoyong, LIU Wenbo, HE Zongbei, WANG Yifan, YUN Di |
| 图7 引入平流通量后3个颗粒烧结时的形貌演化过程 |
| Fig.7 Simulated evolutions of three particles by the phase-field methods of advection flux (a) 0 step (b) 2 × 104 step (c) 4 × 104 step (d) 6 × 104 step |
|