UN核燃料烧结致密化过程的相场模拟 |
| 戚晓勇, 柳文波, 何宗倍, 王一帆, 恽迪 |
|
Phase-Field Simulation of the Densification Process During Sintering of UN Nuclear Fuel |
| QI Xiaoyong, LIU Wenbo, HE Zongbei, WANG Yifan, YUN Di |
| 图5 平流通量对2个颗粒烧结过程中晶界气孔演化的影响 |
| Fig.5 Simulated evolutions of a pore in the grain boundary between two particles by the phase-field methods of without (a-c) and with (d-f) advection flux (a, d) 10 × 104 step (b, e) 20 × 104 step (c, f) 30 × 104 step |
|