机器学习辅助2000 MPa级弹簧钢成分和热处理工艺开发 |
| 杨累, 赵帆, 姜磊, 谢建新 |
|
Development of Composition and Heat Treatment Process of 2000 MPa Grade Spring Steels Assisted by Machine Learning |
| YANG Lei, ZHAO Fan, JIANG Lei, XIE Jianxin |
| 图20 奥氏体的TEM明场像和选区电子衍射花样 |
| Fig.20 TEM bright field image and selected area electron diffraction pattern (inset) of austenite indicated by arrows |
|