机器学习辅助2000 MPa级弹簧钢成分和热处理工艺开发 |
| 杨累, 赵帆, 姜磊, 谢建新 |
|
Development of Composition and Heat Treatment Process of 2000 MPa Grade Spring Steels Assisted by Machine Learning |
| YANG Lei, ZHAO Fan, JIANG Lei, XIE Jianxin |
| 图19 1#钢和2#钢在不同温度回火后的拉伸曲线 |
| Fig.19 Tensile curves of samples with different tempering temperatures (a) 1# steel (b) 2# steel |
|