机器学习辅助2000 MPa级弹簧钢成分和热处理工艺开发 |
| 杨累, 赵帆, 姜磊, 谢建新 |
|
Development of Composition and Heat Treatment Process of 2000 MPa Grade Spring Steels Assisted by Machine Learning |
| YANG Lei, ZHAO Fan, JIANG Lei, XIE Jianxin |
| 图13 回火温度对力学性能的影响 |
| Fig.13 Effects of tempering temperature on mechanical properties (a) tensile and yield strengths (b) elongation at break and reduction in area (c) prediction results of the C2P model |
|