机器学习辅助2000 MPa级弹簧钢成分和热处理工艺开发 |
| 杨累, 赵帆, 姜磊, 谢建新 |
|
Development of Composition and Heat Treatment Process of 2000 MPa Grade Spring Steels Assisted by Machine Learning |
| YANG Lei, ZHAO Fan, JIANG Lei, XIE Jianxin |
| 图7 1#钢和2#钢在不同温度淬火后显微组织的SEM像 |
| Fig.7 SEM images of 1# steel (a-c) and 2# steel (d-f) after quenching at 870oC (a, d), 910oC (b, e), and 950oC (c, f) (Insets show the enlarged images) |
|