机器学习辅助2000 MPa级弹簧钢成分和热处理工艺开发 |
| 杨累, 赵帆, 姜磊, 谢建新 |
|
Development of Composition and Heat Treatment Process of 2000 MPa Grade Spring Steels Assisted by Machine Learning |
| YANG Lei, ZHAO Fan, JIANG Lei, XIE Jianxin |
| 图5 抗拉强度和伸长率的样本数据和MLDS设计结果 |
| Fig.5 Tensile strength and elongation of sample data and design results obtained by the MLDS (a) all data (b) magnification of design results area for rectangle zone in Fig.5a |
|