高铁转向架用钢G390NH在模拟海洋和工业大气环境下的腐蚀行为及产物演化规律 |
| 宋嘉良, 江紫雪, 易盼, 陈俊航, 李曌亮, 骆鸿, 董超芳, 肖葵 |
|
Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment |
| SONG Jialiang, JIANG Zixue, YI Pan, CHEN Junhang, LI Zhaoliang, LUO Hong, DONG Chaofang, XIAO Kui |
| 图9 3.5%NaCl环境中不同周期腐蚀产物XRD谱 |
| Fig.9 XRD spectra of corrosion products in different periods in 3.5%NaCl environment (a) 24 h (b) 120 h (c) 240 h (d) 360 h |
|