高铁转向架用钢G390NH在模拟海洋和工业大气环境下的腐蚀行为及产物演化规律 |
| 宋嘉良, 江紫雪, 易盼, 陈俊航, 李曌亮, 骆鸿, 董超芳, 肖葵 |
|
Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment |
| SONG Jialiang, JIANG Zixue, YI Pan, CHEN Junhang, LI Zhaoliang, LUO Hong, DONG Chaofang, XIAO Kui |
| 图1 G390NH显微组织的OM像 |
| Fig.1 OM image of microstructure for G390NH |
|