600℃ NaCl盐雾环境下GH4169合金的腐蚀行为 |
| 张伟东, 崔宇, 刘莉, 王文泉, 刘叡, 李蕊, 王福会 |
|
Corrosion Behavior of GH4169 Alloy in NaCl Solution Spray Environment at 600oC |
| ZHANG Weidong, CUI Yu, LIU Li, WANG Wenquan, LIU Rui, LI Rui, WANG Fuhui |
| 图9 GH4169合金在600℃下NaCl盐雾环境腐蚀20 h后腐蚀产物膜的TEM像、SAED花样及Cl元素线分布结果 |
| Fig.9 TEM image and corresponding SAED patterns of the corrosion scale of GH4169 alloy exposed in NaCl solution spray at 600oC for 20 h (a), and Cl element distribution along the EDS-line in Fig.9a (b) |
|