600℃ NaCl盐雾环境下GH4169合金的腐蚀行为 |
| 张伟东, 崔宇, 刘莉, 王文泉, 刘叡, 李蕊, 王福会 |
|
Corrosion Behavior of GH4169 Alloy in NaCl Solution Spray Environment at 600oC |
| ZHANG Weidong, CUI Yu, LIU Li, WANG Wenquan, LIU Rui, LI Rui, WANG Fuhui |
| 图8 GH4169合金在600℃的NaCl盐雾环境中腐蚀100 h后截面的EPMA元素面分布图 |
| Fig.8 EPMA maps of the elemental distribution of the cross-section of GH4169 alloy exposed in NaCl solution spray environment at 600oC for 100 h |
|