600℃ NaCl盐雾环境下GH4169合金的腐蚀行为 |
| 张伟东, 崔宇, 刘莉, 王文泉, 刘叡, 李蕊, 王福会 |
|
Corrosion Behavior of GH4169 Alloy in NaCl Solution Spray Environment at 600oC |
| ZHANG Weidong, CUI Yu, LIU Li, WANG Wenquan, LIU Rui, LI Rui, WANG Fuhui |
| 图7 GH4169合金在600℃固态NaCl + 含O2水蒸汽和NaCl盐雾环境下腐蚀20 h后截面的EPMA元素面分布图 |
| Fig.7 EPMA maps of the elemental distribution of the cross-section of GH4169 alloy exposed in solid NaCl in wet O2 (a) and NaCl solution spray (b) environments at 600oC for 20 h |
|