Ti6Al4V表面微纳结构的制备及生物活性 |
| 高晗, 刘力, 周笑宇, 周心怡, 蔡汶君, 周泓伶 |
|
Preparation and Bioactivity of Micro-Nano Structure on Ti6Al4V Surface |
| GAO Han, LIU Li, ZHOU Xiaoyu, ZHOU Xinyi, CAI Wenjun, ZHOU Hongling |
| 图3 Ti6Al4V经SLA + IHT得到的多级结构在模拟体液浸泡14 d前后的XRD谱 |
| Fig.3 XRD spectra of Ti6Al4V after SLA + IHT and soaking in SBF for 14 d (SLA represents the process of sandblasting + (36%~38%)HCl acid etching for 10 min with ultrasonic treatment, SBF—simulated body fluid, IHT—induction heating treatment, HA—hydroxyapatite) |
|