Nd90Al10 晶界调控对晶界扩散磁体磁性能和微观结构的影响 |
| 刘路军, 刘政, 刘仁辉, 刘永 |
|
Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process |
| LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong |
| 图5 AMG磁体的高角环形暗场(HAADF)像及选区电子衍射(SAED)花样 |
| Fig.5 High-angle annular dark field (HAADF) image (a) and SAED patterns of area A (b) and area B (c) of AMG magnet (1: Nd2Fe14B, 2: Tb-rich shell, 3: Nd-rich phase) (Inset in Fig.5b shows the interplanar spacing) |
|