一种含富锰偏析带的热轧临界退火中锰钢的组织调控及强化机制 |
| 陈学双, 黄兴民, 刘俊杰, 吕超, 张娟 |
|
Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band |
| CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan |
| 图10 计算的3种临界退火态中锰钢中偏析带在拉伸后的马氏体转变率 |
| Fig.10 Calculated martensite transformation ratios of segregation band in IA600, IA650, and IA700 samples |
|