一种含富锰偏析带的热轧临界退火中锰钢的组织调控及强化机制 |
| 陈学双, 黄兴民, 刘俊杰, 吕超, 张娟 |
|
Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band |
| CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan |
| 图9 IA650中样品中偏析带在拉伸前后的SEM像 |
| Fig.9 SEM images of segregation band in IA650 sample before (a) and after (b) tension (The arrows and circle represent the segregation area before and after tension, respectively) |
|