一种含富锰偏析带的热轧临界退火中锰钢的组织调控及强化机制 |
| 陈学双, 黄兴民, 刘俊杰, 吕超, 张娟 |
|
Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band |
| CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan |
| 图8 IA600和IA700样品拉断后的相分布图和IPF |
| Fig.8 EBSD phase maps (a, c) and IPFs (b, d) of IA600 (a, b) and IA700 (c, d) samples after tensile deformation |
|