一种含富锰偏析带的热轧临界退火中锰钢的组织调控及强化机制 |
| 陈学双, 黄兴民, 刘俊杰, 吕超, 张娟 |
|
Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band |
| CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan |
| 图3 临界退火态中锰钢拉伸前后的XRD谱和奥氏体含量 |
| Fig.3 XRD spectra (a) and retained austenite (RA) contents (b) of inter-critical annealed mendium-Mn steels before and after tensile deformation |
|