轧制态Mg-xZn-0.5Er合金板材组织及室温成形性能 |
| 娄峰, 刘轲, 刘金学, 董含武, 李淑波, 杜文博 |
|
Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature |
| LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo |
| 图4 变形量为78%时轧制态Mg-xZn-0.5Er合金RD-TD面微观组织的OM像 |
| Fig.4 OM images of as-rolled Mg-0.5Zn-0.5Er (a), Mg-2.0Zn-0.5Er (b), Mg-3.0Zn-0.5Er (c), and Mg-4.0Zn-0.5Er (d) alloys on the RD-TD plane with thickness reduction of 78% |
|