轧制态Mg-xZn-0.5Er合金板材组织及室温成形性能 |
| 娄峰, 刘轲, 刘金学, 董含武, 李淑波, 杜文博 |
|
Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature |
| LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo |
| 图1 轧制态Mg-xZn-0.5Er (x = 0.5、2.0、4.0)合金不同变形量下轧向-横向(RD-TD)面微观组织的OM像 |