自然时效对Al-2.95Cu-1.55Li-0.57Mg-0.18Zr合金160℃人工时效的影响 |
| 巩向鹏, 伍翠兰, 罗世芳, 沈若涵, 鄢俊 |
|
Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC |
| GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun |
| 图9 160℃双级时效第二处峰值(192 h)试样的HAADF-STEM像 |
| Fig.9 HAADF-STEM images of the second-peak-aged T66 sample at 192 h (a) morphology of precipitates viewed along the [001]Al direction (Inset is the atomic-resolution HAADF image of a lath-like S precipitate) (b) morphology of T1 precipitates viewed along [110]Al direction (Inset is the atomic-resolution HAADF image of a T1 precipitate) |
|