自然时效对Al-2.95Cu-1.55Li-0.57Mg-0.18Zr合金160℃人工时效的影响 |
| 巩向鹏, 伍翠兰, 罗世芳, 沈若涵, 鄢俊 |
|
Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC |
| GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun |
| 图5 自然时效7 d试样中原子团簇的3DAP分析 |
| Fig.5 3DAP analyses of atomic clusters in the sample which is natural aged for 7 d (dpair—distance between nearest-neighbor atoms) (a) nearest-neighbor analysis of Mg (b) nearest-neighbor analysis of Cu (c) distribution of Mg clusters and Mg-Cu co-clusters |
|