自然时效对Al-2.95Cu-1.55Li-0.57Mg-0.18Zr合金160℃人工时效的影响 |
| 巩向鹏, 伍翠兰, 罗世芳, 沈若涵, 鄢俊 |
|
Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC |
| GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun |
| 图1 合金经单、双级时效处理后的力学性能 |
| Fig.1 Mechanical properties of the alloys with T6 and T66 treatment (a) age-hardening curves vs aging time (b) engineering stress-strain curves of peak-aged T6 alloys at 96 and 192 h, respectively (c) engineering stress-strain curves of peak-aged T66 alloys at 96 and 192 h, respectively (d) diagram of tensile properties |
|