NiTi-Nb原位复合材料的准线性超弹性变形 |
| 姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山 |
|
Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite |
| JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan |
| 图6 NiTi-Nb复合材料在6次加载过程中的应力-应变曲线,以及在加载过程中NiTi马氏体峰面积随宏观应变的演变曲线 |
| Fig.6 Stress-strain curves of the as-annealed NiTi-Nb composite, and the corresponding B19'-NiTi(001) peak area curves in the 6 loading processes (In each loading process, the “first yield point” on the stress-strain curve just corresponds to the “turning point” on the evolution curve of B19' peak areas, as marked by each dash line) |
|