应力比对含缺陷选区激光熔化TC4合金稳态疲劳裂纹扩展速率的影响 |
||||||||||||
| 戚钊, 王斌, 张鹏, 刘睿, 张振军, 张哲峰 | ||||||||||||
|
Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects |
||||||||||||
| QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng | ||||||||||||
| 表1 SLM TC4合金的拉伸性能 |
||||||||||||
| Table 1 Mechanical properties of SLM TC4 alloy |
||||||||||||
|
||||||||||||