应力比对含缺陷选区激光熔化TC4合金稳态疲劳裂纹扩展速率的影响 |
| 戚钊, 王斌, 张鹏, 刘睿, 张振军, 张哲峰 |
|
Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects |
| QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng |
| 图2 2种选区激光熔化(SLM) TC4合金的OM像 |
| Fig.2 OM images of selective laser melting (SLM) TC4 alloy (a) SD specimen (laser power is 300 W, scanning speed is 1200 mm/s) (b) LD specimen (laser power is 250 W, scanning speed is 1400 mm/s) |
|