W含量对Ti-42Al-5Mn-xW合金相转变行为的影响
李小兵, 潜坤, 舒磊, 张孟殊, 张金虎, 陈波, 刘奎

Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy
LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui
图3 W含量对Ti-42Al-5Mn-xW合金特征相变温度的影响
Fig.3 Effects of W concentration on the phase transformation temperature in Ti-42Al-5Mn-xW (The data of Ti-42Al-5Mn is quoted from Ref.[14]. Teut—eutectoid reaction temperature, Tγ-solv—γ phase solvus temperature, Tβ —β-phase single region temperature)