| Continuous casting | Main related parameter | Sample size of |
|---|
| parameter | | filtered dataset | | Casting speed | Oscillation frequency, Qstopper, Qnozzle, and immersion depth | 141 | | Immersion depth | Mold level | 1440 | | Mold level | Immersion depth | 1253 | | Oscillation frequency | Casting speed, Qstopper, position of stopper, immersion depth, and total water flow rate | 54 | | Slab width | Total water flow rate, oscillation frequency, Qshield, and immersion depth | 1670 | | Position of stopper | Qstopper, Qnozzle, immersion depth, and superheat | 612 | | Qstopper | Qnozzle, total water flow rate, superheat, Qshield, and casting speed | 102 | | Qnozzle | Qstopper, slab width, and superheat | 417 | | Qshield | Qnozzle and total water flow rate | 1123 | | Superheat | Qnozzle and immersion depth | 369 | | Total water flow rate | Slab width, Qshield, and superheat | 2727 | | Mold taper | Total water flow rate | 3517 |
|