珠光体-奥氏体相变中扩散通道的相场法研究 |
| 李赛, 杨泽南, 张弛, 杨志刚 |
|
Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation |
| LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang |
| 图12 奥氏体/珠光体界面迁移速率随界面扩散激活能(Qint)的变化趋势 |
| Fig.12 Variation of the migration rate of P/γ boundary with the activity energy of interfacial diffusion (Qint), where the circle point is the calculated value and the diamond point is the experimental estimated value |
|