珠光体-奥氏体相变中扩散通道的相场法研究 |
| 李赛, 杨泽南, 张弛, 杨志刚 |
|
Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation |
| LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang |
| 图11 合金元素在奥氏体和铁素体中的扩散通量分布 |
| Fig.11 Distributions of the fluxes of C in austenite/ferrite held at 740oC (a) and Mn in austenite/ferrite held at 720oC (b) along the austenite/pearlite boundary |
|