珠光体-奥氏体相变中扩散通道的相场法研究 |
| 李赛, 杨泽南, 张弛, 杨志刚 |
|
Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation |
| LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang |
| 图10 考虑γ + α扩散通道时,奥氏体/珠光体界面前沿合金元素浓度分布 |
| Fig.10 Distributions of the alloy element beside the austenite/pearlite boundary with the γ + α diffusional path (a-c) the simulated morphology (a) and C profiles in austenite (b) and ferrite (c) in group B (d-f) the simulated morphology (d) and C profiles in austenite (e) and ferrite (f) in group E (g-i) the simulated morphology (g) and Mn profiles in austenite (h) and ferrite (i) in group H |
|