珠光体-奥氏体相变中扩散通道的相场法研究 |
| 李赛, 杨泽南, 张弛, 杨志刚 |
|
Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation |
| LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang |
| 图8 初始珠光体在720℃等温3.81 s时的浓度分布 |
| Fig.8 C (a) and Mn (b) distributions in the austenite held at 720oC for 3.81 s |
|