珠光体-奥氏体相变中扩散通道的相场法研究 |
| 李赛, 杨泽南, 张弛, 杨志刚 |
|
Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation |
| LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang |
| 图6 等温温度为720℃时,珠光体-奥氏体相变组织形貌演化 |
| Fig.6 Microstructural evolutions of the pearlite-austenite transformation at 720oC with the 150 nm-spacing layer of the initial pearlite, the diffusional paths are γ + α + interface (a-c), γ + α (d-f), and γ (g-i), respectively |
|