GH3600镍基高温合金极薄带的制备及尺寸效应 |
||||||||||||||||||||
| 于少霞, 王麒, 邓想涛, 王昭东 | ||||||||||||||||||||
|
Preparation and Size Effect of GH3600 Nickel-Based Superalloy Ultra-Thin Strips |
||||||||||||||||||||
| YU Shaoxia, WANG Qi, DENG Xiangtao, WANG Zhaodong | ||||||||||||||||||||
| 表2 0.07 mm厚GH3600镍基高温合金带材屈服强度、抗拉强度、延伸率随带材厚度/平均晶粒尺寸(T / D)的变化 |
||||||||||||||||||||
| Table 2 Variations of yield strength, tensile strength, and elongation of 0.07 mm thick GH3600 nickel-based superalloy strips with strip thickness/average grain size (T / D) |
||||||||||||||||||||
|
||||||||||||||||||||