GH3600镍基高温合金极薄带的制备及尺寸效应 |
| 于少霞, 王麒, 邓想涛, 王昭东 |
|
Preparation and Size Effect of GH3600 Nickel-Based Superalloy Ultra-Thin Strips |
| YU Shaoxia, WANG Qi, DENG Xiangtao, WANG Zhaodong |
| 图5 800℃退火后不同厚度GH3600镍基高温合金带材的晶粒取向散布(GOS)图 |
| Fig.5 Grain orientation spread (GOS) diagrams of GH3600 nickel-based superalloy strips with different thicknesses after annealing at 800oC (a) 0.25 mm (b) 0.125 mm (c) 0.07 mm |
|