前置渗氧对TC4钛合金低温等离子复合渗层微观结构和耐磨损性能的影响 |
| 王海峰, 张志明, 牛云松, 杨延格, 董志宏, 朱圣龙, 于良民, 王福会 |
|
Effect of Pre-Oxidation on Microstructure and Wear Resistance of Titanium Alloy by Low Temperature Plasma Oxynitriding |
| WANG Haifeng, ZHANG Zhiming, NIU Yunsong, YANG Yange, DONG Zhihong, ZHU Shenglong, YU Liangmin, WANG Fuhui |
| 图10 不同工艺渗层的磨痕形貌 |
| Fig.10 Low (a-c) and high (d-f) magnified wear trace morphologies of coatings obtained by different processes (a, d) PN 3h (b, e) PO+PN 3h (c, f) PO+PN 4h |
|