多相Ni3Al基高温合金微区氧化行为 |
| 胡敏, 周生玉, 国京元, 胡明昊, 李冲, 李会军, 王祖敏, 刘永长 |
|
Oxidation Behavior of Micro-Regions in Multiphase Ni3Al-Based Superalloys |
| HU Min, ZHOU Shengyu, GUO Jingyuan, HU Minghao, LI Chong, LI Huijun, WANG Zumin, LIU Yongchang |
| 图7 枝晶干γ' + γ在1000℃氧化10 min后截面形貌的TEM像、选区电子衍射(SAED)花样以及框线区域的EDS元素面扫分布 |
| Fig.7 Cross-sectional TEM image of γ' + γ dendrite oxidized at 1000oC for 10 min (a) and the EDS element mapping of the frame area depicting the distributions of elements O (b), Al (c), Cr (d), Fe (e), and Ni (f) (Inset in Fig.7a shows the selected area electron diffraction (SAED) pattern of γ' + γ dendrite) |
|