Ni-Ir/Al2O3 负载型催化剂的制备及其用于水合肼分解制氢性能 |
| 杜宗罡, 徐涛, 李宁, 李文生, 邢钢, 巨璐, 赵利华, 吴华, 田育成 |
|
Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine |
| DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng |
| 图10 Ni60Ir40/Al2O3催化N2H4·H2O分解制氢循环耐久性测试曲线和反应前后催化剂的H2-TPD曲线 |