Ni-Ir/Al2O3 负载型催化剂的制备及其用于水合肼分解制氢性能
杜宗罡, 徐涛, 李宁, 李文生, 邢钢, 巨璐, 赵利华, 吴华, 田育成

Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine
DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng
图7 不同浓度N2H4·H2O催化分解生成的气体体积(VH2+N2)与时间线性关系曲线,N2H4·H2O浓度对Ni60Ir40/Al2O3在303 K条件下催化分解反应制氢速率的影响,以及高、低浓度条件下lnr与ln[N2H4·H2O]的拟合关系
Fig.7 Time profiles for the total gas volume (VH2+N2) from the catalytic decomposition of N2H4·H2O solutions with varied concentrations (a), effects of N2H4·H2O concentration on its initial reaction rate in the presence of Ni60Ir40/Al2O3 at 303 K (b), and plots of lnrvs ln[N2H4·H2O] with low (c) and high (d) N2H4·H2O concentrations